High Conductivity
Electrolytic Copper Rods & Tubes
As per BA 2874—1969, C
101
BS 1977—1963 (Tubes)
CHEMICAL REQUIREMENTS
Copper ..
.. ..
99.9%-min.(inclusive
of silver)
Lead ..
.. ..
0.005%
Total
impurities ..
.. ..
0.03% (excluding
oxygen)
PHYSICAL PROPERTIES
Tensile strength ..
.. ..
23 to 35 kgs/mm2
Elongation ..
.. ..
55 to 6%
Electrical conductivity at 200C
.. ..
101% IACS (annealed)
FABRICATION
PROPERTIES
Capacity for being cold worked
.. .. ..
Poor
Hot
formed .. .. ..
Good
Machine ability .. ..
..
35
Suitability for silver brazing ..
.. ..
Fair
Soldering ..
.. ..
Poor
(In
an inert or slightly oxidizing condition.)
USES
Electrical conductors
switches, terminals, gaskets, radiators, cotter
pins, nails, rivets, tubes etc., requiring high
electrical/thermal conductivity
-
Material can
be supplied in any temper as required by
customers.
|